Typically the outer layer is a thin fiberglass sheet followed by luann plywood insulating foam board and an inner layer of paneling or pressed cardboard.
Rv fiberglass siding delamination.
One method of fixing this damage can be through using a de lamination kit.
Average coverage is 8 12 square feet coverage for the 12 rv delamination repair kit up to 30 square feet with the 24 rv delamination repair kit.
This situation may not be noticeable right away.
What are rv walls made of.
We will always go with the compset slv if we have to make a repair.
The result is a convex air pocket that causes bonding agent failure and separation.
They re normally held together by a strong adhesive which provides much of the rv s structural strength.
This damage can occur through water leaks or hard impacts.
A bubble forms over the unglued pocket which will grow in size over time as the fiberglass walled rv flexes with normal use.
I successfully completed the delamination repair on my 11 year old rv and it looks great now.
Rv siding delamination repair.
In your case of delamination on the front of an rv i would recommend replacing the entire front as it is a relatively small area and the cost to replace versus repair if the damaged area is small is insignificant especially when you consider the integrity of the repair.
Simply put de lamination occurs when the bonding agent holding the fiberglass siding to its backing is damaged and it lets go of its hold.
The proprietary composet slv epoxy system works on re bonding delaminated fiberglass wall panels on rv s motorhomes campers trailers 5th wheels and toy haulers.
Walk around the rv and pay attention to the side front and rear walls.
The bubble will gradually crack and trap moisture inside causing further damage.
Having a styrofoam safe product is also a requirement for re bonding delamination on rv fiberglass siding walls roofs floors.
The fiberglass should be flat and smooth.
This rv delamination problem is obvious.
We are available almost 24 7 to answer questions.
If you are shopping for a used rv it s critical to know what rv sidewall delamination looks like.
Testing parameters included work life gel time fixture strength viscocity etc.
You apparently have what s called sidewall delamination due to water intrusion.
Here are my top tips and tricks i learned that may help you wit.
If you notice any waves bubbles or creases in the sidewalls you are looking at rv sidewall delamination.